• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Cyanide leaching gold fingers and CPUs

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Fellows,

I am not dead nor anyone else that came close to my plant, I did recover 2.53 grams of gold from 950 g of mixed CPUs. Also used the method desrcibed here, addition of 30% peroxide to rinse everything which was inside the cyanide leach, and added chlorine at pH 9 followed by NaOH to convert left over cyanide solution to cyanate.

I have repeatedly asked for consultant on setting up a full WEEE recycling plant but no one responded, so it is not I am not looking for professionals in this field who could get paid for their consultancy.

Again, I do have the capitals to start a 1 ton per day WEEE recycling plant, then either go to EW process to recover values, or ship to smelting company.


Regards,
Kevin
 