Hi, after a very clean drop with SMB (right pic), I washed the gold with HCl and was surprised to see what appears to be some gold redissolving (left pic solution removed from gold). I did not do a water wash first, and wish I had. I did have to use a small amount, 3gm, of sulfamic acid after AR if that matters.
Stannous test appears to be positive, but with a small sample in a test tube gold does not drop with SMB or copperas.
Question 1. Is there gold in solution or other contamination giving false positive?
Question 2. How did HCl dissolve gold? Obviously there would have to be some oxidizer in there. Did the nitric regenerate somehow? Or my beaker cover was not cleaned thoroughly and maybe there were some nitrates on it that condensed down into the breaker?
Question 3. How do I proceed? I think I'm going to try to drop the whole thing with SMB.
Thank you for your help, Vinny
Stannous test appears to be positive, but with a small sample in a test tube gold does not drop with SMB or copperas.
Question 1. Is there gold in solution or other contamination giving false positive?
Question 2. How did HCl dissolve gold? Obviously there would have to be some oxidizer in there. Did the nitric regenerate somehow? Or my beaker cover was not cleaned thoroughly and maybe there were some nitrates on it that condensed down into the breaker?
Question 3. How do I proceed? I think I'm going to try to drop the whole thing with SMB.
Thank you for your help, Vinny