Are you trying to strip the cable to take to the scrapyard or are you trying to repurpose it for something else.What solvent is best for dissolving polyethylene on the outside of rf cables?
Neither. I’m trying to get the cut off piece out of the connector. Without removing any gold.Are you trying to strip the cable to take to the scrapyard or are you trying to repurpose it for something else.
Theoretically, high molecular weight polyethylene dissolves in hot non-polar solvents at temperatures above 200°C. But in practice... acetone, toluene, benzene, dibutyl phthalate, dichloroethane, chloroform, carbon tetrachloride, kerosene, isopropyl alcohol, methyl alcohol, ethyl alcohol, xylene, hexane, turpentine - does not dissolveWhat solvent is best for dissolving polyethylene on the outside of rf cables?
How about a knife stripping tool? Start it through a jig, then pull it through. A drum/winch if you have a lot of it. No toxic chemicals necessary.Neither. I’m trying to get the cut off piece out of the connector. Without removing any gold.
What kind of connector? You may be able to cut trough it with bench shears along the length of the pin, releasing it.Neither. I’m trying to get the cut off piece out of the connector. Without removing any gold.
A little bit of heat softens the plastic. Don't need to combust, just get to a very pliable state.Neither. I’m trying to get the cut off piece out of the connector. Without removing any gold.
What solvent is best for dissolving polyethylene on the outside of rf cables?
We do NOT recommend using Piranha solution for anything in refining.Hydrogen peroxide with sulphuric acid
Welcome to us by the way.Hydrogen peroxide with sulphuric acid
Thank you for your valuable suggestions...I will follow up this in futureWelcome to us by the way.
Here are some thing for your studies.
Make special attention to the Safety section and dealing with waste.
Hokes book needs to be read several times.
We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/
Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/
Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
Welcome to us by the way.
Here are some thing for your studies.
Make special attention to the Safety section and dealing with waste.
Hokes book needs to be read several times.
We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/
Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/
Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
Bang bang Maxwell Silver Hammer came down on his... RF cable... ... Doesn't quite have the same ring to it as the original. ;DAhhh... Mr. Hammer! One of my favorite tools when breaking things down. Primitive, but highly effective.
Dave
Yes, indeed. The hammer. Probably the most emotionally satisfying tool ever created. Useful, too.Ahhh... Mr. Hammer! One of my favorite tools when breaking things down. Primitive, but highly effective.
Dave
It's a great way to end a bad dayYes, indeed. The hammer. Probably the most emotionally satisfying tool ever created. Useful, too.
Time for more coffee.
Yep, and if all else fails get a bigger hammer. That is how you fit a square peg in a round hole.Yes, indeed. The hammer. Probably the most emotionally satisfying tool ever created. Useful, too.