What is the other way?
Very slow way. I did small scale experiments with nitric and found if I score each end and use very diluted nitric acid I don’t even have to mess with the cables. Just dissolve the entire connector. It does dissolve a ting bit of the plating off but I’m not worried. I’ll get it later.
 
Haha. Thanks for the advice but I’ve found a different way.
Are you going to share what worked for you?

Edit to add: My eyes were not fully functional when I replied, I did not see that it was already answered. ;)
 