About to process these CPUs with the heat sinks on them does anyone have any idea of the yield I should expect? So I know I'm close to average yield when I process these.
 

Attachments

  • 16389990766378047902960483949888.jpg
    16389990766378047902960483949888.jpg
    4.5 MB · Views: 45
hi bro
this type of ceramic cpu gold quntity is 0.1g per cpu, you can get 1g gold from 9 cpus
I agree. And will add, IF you get a full recovery. Even the braze under the silica chip. The chip has to slide free of the body or there will still be gold left behind.
 