Hello everyone
During work one patch was unusual
After pretreatment and AR dissolving when adding SMB the whole patch turned to white ppt
I filtered it and separated the precipitate.

It looks like fiber material
By searching it can't be metastannic or palladium ( i think)
Any suggestions about it
It is in
first container in the video
 

Attachments

  • IMG_20241102_094535.jpg
    IMG_20241102_094535.jpg
    2.6 MB
  • IMG_20241102_094552.jpg
    IMG_20241102_094552.jpg
    2.5 MB
Last edited:
Sorry i don't know how to upload videos here is gif
 

Attachments

  • VID_20241101_202804[ConvGif].gif
    VID_20241101_202804[ConvGif].gif
    3.9 MB
Slag from gold-laden carbon
Pretreatment with nitric acid
By the way they ashed the carbon before smelting
Same stuff as before.
It is impossible to say what it is without testing.
I'd guess some kind of insoluble Sulfite or complex thereof since it emerges with SMB.
 
So can i use copper cementation with such dirty Pregnant AR solution to precipitate gold
 