Drowningbodacius
Well-known member
So I finally did and completes ky first recovery. Thanks everyone on The forum for answering all my questions. I recovered 1.3g from fifty Intel and cpu chips using same method of getting them off the board and using a ap soak. Is this the normal trips off that much or is it possible that I have some in ky ap solution? I'm just wondering as it was my first recovery