Slochteren
Well-known member
Hi,
after dropping Gold with smb i have some gold floating on top of it, i read on the forum somewhere how to solve this but cannot find it back. Suggestions?
Thanks Paul
after dropping Gold with smb i have some gold floating on top of it, i read on the forum somewhere how to solve this but cannot find it back. Suggestions?