Samir Das Gupta
Member
- Joined
- Mar 3, 2025
- Messages
- 6
All gold plated components arent the same. Many gold plated components are often blended with cobalt or nickel which makes dissolution/ recovery longer/ more expensive/ less efficient. Also, plated gold tends to be harder to dissolve than ore gold. The typical alkaline: amino acid: oxidant formula that works on ore may not work as well on e waste. Lots of experimenting required to perfect it and even then it requires to be tweaked constantly.
When excess amino/ glycine is required then its feasible only when the manufacturing system incorporates the re-use of the excess amino acid otherwise the cost can be greater than the recovered gold.
Has anyone worked on electrolysis/ electrowinning dissolved gold glycinate instead of carbon leaching? Sounds like a cleaner process.
When excess amino/ glycine is required then its feasible only when the manufacturing system incorporates the re-use of the excess amino acid otherwise the cost can be greater than the recovered gold.
Has anyone worked on electrolysis/ electrowinning dissolved gold glycinate instead of carbon leaching? Sounds like a cleaner process.