Hi all,
Not sure if this has been discussed before but I haven't been able to come up with a search that helps find the solution.

I'm trying to attempt to precipitate a very stubborn solution of metals that lurked in a 350g batch of mostly 1/10 10k gold filled.
The color is greenish brown, which I assume is mostly copper, iron, and/or nickel.
No reasonable amount of SMB (stumpout) was dropping all the gold. I got some to drop but it was way under what's expected. Stannous test is positive.
Today, I put some copper pipe and solid copper wire in the solution on a hot plate at 80c but a pretty tenacious black precipitate is coating it. After two hours, little copper has dissolved, likely because of passivation.
If this has been covered/explained, I'd be grateful for the link. Otherwise:

1. Please share what you think I'm dealing with and where I went wrong
2. What might I do to force the gold to drop so I can re-refine.

How I got here (if it matters)
350g gold filled jewelry heated to redness in a melt dish under torch into large beaker with small nitric boils. Did that until the nitric was clear. Magnet test noted some magnetic items were still in there. If you ever refined GF, it's not ever pretty the first round. I removed all small magnetic items like screws, springs, etc. that I found though.
I didn't weigh the items before adding HCL, which I think is a good step (as if I had, say, 60g I could rethink my process since I'm expecting to leave the nitric boil phase with <35).

Got it to dissolve with HCL and nitric, added sulfuric, filtered. Added SMB. Strong reaction. Kept going... I suspected too much nitric, added maybe 2 heaping tsp of sulfamic crystals and added heat. Stir /w stir bar till dissolved, then cooled to room temperature. Started again with SMB. Went through half a bottle of stumpout. Slept on it.

The next day, I started evaporating. When it dried it was like concrete. My stir bar was now a fossil. Started reconstituting using HCL and distilled water. When done, saw a precipitate on the bottom of the beaker. Stannous test is positive. The color is so horrible I only could guess it was gold so I decanted after a day of settling and actually located maybe 5-10g. It looked pretty decent.

I saw a post from January where someone was having issues getting their gold to drop, and the hail Mary was to add copper start over.

So as I said above, the copper is in and I'm currently slowly doing another evaporation round. As of my writing this, stannous test is still positive. Note, I've not re-filtered the solution after reconstituting, and it's still clear.

Thanks in advance for any help!
 
Hi all,
Not sure if this has been discussed before but I haven't been able to come up with a search that helps find the solution.

I'm trying to attempt to precipitate a very stubborn solution of metals that lurked in a 350g batch of mostly 1/10 10k gold filled.
The color is greenish brown, which I assume is mostly copper, iron, and/or nickel.
No reasonable amount of SMB (stumpout) was dropping all the gold. I got some to drop but it was way under what's expected. Stannous test is positive.
Today, I put some copper pipe and solid copper wire in the solution on a hot plate at 80c but a pretty tenacious black precipitate is coating it. After two hours, little copper has dissolved, likely because of passivation.
If this has been covered/explained, I'd be grateful for the link. Otherwise:

1. Please share what you think I'm dealing with and where I went wrong
2. What might I do to force the gold to drop so I can re-refine.

How I got here (if it matters)
350g gold filled jewelry heated to redness in a melt dish under torch into large beaker with small nitric boils. Did that until the nitric was clear. Magnet test noted some magnetic items were still in there. If you ever refined GF, it's not ever pretty the first round. I removed all small magnetic items like screws, springs, etc. that I found though.
I didn't weigh the items before adding HCL, which I think is a good step (as if I had, say, 60g I could rethink my process since I'm expecting to leave the nitric boil phase with <35).

Got it to dissolve with HCL and nitric, added sulfuric, filtered. Added SMB. Strong reaction. Kept going... I suspected too much nitric, added maybe 2 heaping tsp of sulfamic crystals and added heat. Stir /w stir bar till dissolved, then cooled to room temperature. Started again with SMB. Went through half a bottle of stumpout. Slept on it.

The next day, I started evaporating. When it dried it was like concrete. My stir bar was now a fossil. Started reconstituting using HCL and distilled water. When done, saw a precipitate on the bottom of the beaker. Stannous test is positive. The color is so horrible I only could guess it was gold so I decanted after a day of settling and actually located maybe 5-10g. It looked pretty decent.

I saw a post from January where someone was having issues getting their gold to drop, and the hail Mary was to add copper start over.

So as I said above, the copper is in and I'm currently slowly doing another evaporation round. As of my writing this, stannous test is still positive. Note, I've not re-filtered the solution after reconstituting, and it's still clear.

Thanks in advance for any help!
If you can't find anything about Gold filled you need to improve your searches.
There are a lot of discussions on this topic.

But the general rule with Gold filled as anything mixed metal is:
Dissolve all the base metals first, then dissolve the Gold.

You have not yet detailed your process, but my guess is too much Nitric.

Cement it on Copper (with agitation) and redissolve the dropped powder for a cleaner drop.
 
You have not yet detailed your process, but my guess is too much Nitric.

Cement it on Copper (with agitation) and redissolve the dropped powder for a cleaner drop.

Hi,
Thanks for taking the time to respond!
As I detailed in my process, excess Nitric was my guess too so I evaporated.
I'm cementing to copper with agitation (per my original post) but the noted black coating is blocking. I can't specifically find any reference to what the passivating substance might be.
 
Hi,
Thanks for taking the time to respond!
As I detailed in my process, excess Nitric was my guess too so I evaporated.
I'm cementing to copper with agitation (per my original post) but the noted black coating is blocking. I can't specifically find any reference to what the passivating substance might be.
Was it white Gold filled?
Evaporating the liquid may not be enough until you evaporate to syrup and add HCl.
 
You did not specifically say you filtered out the solids after the nitric pre treatment. You cannot use too much nitric to dissolve the base metals, slowly add until the reaction stops. Using too much nitric is costly but as you are filtering the liquid before moving on it isn't harmful to the process..

But if you didn't filter off the solids after nitric, as you suspected and Ygg confirmed, you have too much nitric. So the question is, did you filter the insolubles from the nitric dissolve and start fresh with new aqua regia?
 
It wasn't white Gold filled. That was a good check though. I went past syrup to solid, but added HCL to reconstitute. Everything but a little gold went back into solution.
There are just a few things that need to be in place for cementing to work.
Clean Copper, sufficient free acid (HCl) and agitation.
 
You did not specifically say you filtered out the solids after the nitric pre treatment. You cannot use too much nitric to dissolve the base metals, slowly add until the reaction stops. Using too much nitric is costly but as you are filtering the liquid before moving on it isn't harmful to the process..

But if you didn't filter off the solids after nitric, as you suspected and Ygg confirmed, you have too much nitric. So the question is, did you filter the insolubles from the nitric dissolve and start fresh with new aqua regia?
Hi, thanks for the help.
The last nitric boil (pre-treatment) for my gold filled remained un-colored. I poured the solution into a large beaker where I have sterling to consume the nitric acid before putting into my waste stream.
I think my excess nitric was because I didn't pour off all that solution because I wanted to retain the colloidal gold I observed in the bottom. It didn't seem like that much but when I added HCL I didn't need any additional nitric to dissolve the gold. At this point, I surmised that I was at risk for having excess nitric but I've dealt with it before.
I filtered after the AR step till the solution was clarified but the color was very green-brown, as I said. Stannous test was, of course, positive.
New update - I shared my issue with chatgpt and it shared a few possibilities. One that stood out was this:

Iron Compounds: Since some of your jewelry is magnetic, it indicates the presence of iron. Iron can form various oxides and hydroxides that can appear black. When exposed to nitric acid and aqua regia, iron may form black iron oxide (Fe3O4) or hydrated iron oxide (FeO(OH)), which can precipitate and coat the copper.

I prompted chatgpt to give me a treatment for this and got a lengthy (but basically simple) treatment centered around ammonia. I checked Hoke's book and verified that it should work. I'll divide a small amount of the solution for experimentation and report the results.
 
I'm gonna add my 2 cents on this old post...if I may. Anytime I did gold filled items, I used a inquartation calculator and melted the gf items with clean copper wire. Then poured the molten mix into a metal pan/ bucket filled with water and made " corn flakes". Then processed with acid of choice to remove base metals...anyhow, always had/ got a good return.
 
I'm gonna add my 2 cents on this old post...if I may. Anytime I did gold filled items, I used a inquartation calculator and melted the gf items with clean copper wire. Then poured the molten mix into a metal pan/ bucket filled with water and made " corn flakes". Then processed with acid of choice to remove base metals...anyhow, always had/ got a good return.
Always a good method.
 
I'm gonna add my 2 cents on this old post...if I may. Anytime I did gold filled items, I used a inquartation calculator and melted the gf items with clean copper wire. Then poured the molten mix into a metal pan/ bucket filled with water and made " corn flakes". Then processed with acid of choice to remove base metals...anyhow, always had/ got a good return.
Thanks for sharing; it resonated with me. I think about melting to shot every time I do this - I don't know what further diluting the material might do though, it's already 1-2k equivalent by volume.
But running acid through a more homogenous material of shot might solve some of my AR-stage issues processing GF - specifically because if I have a really lovely thick coating of gold on an item it might not be affected by the nitric boils, and causes lots of problems because I have very dirty AR.
 
Thanks for sharing; it resonated with me. I think about melting to shot every time I do this - I don't know what further diluting the material might do though, it's already 1-2k equivalent by volume.
But running acid through a more homogenous material of shot might solve some of my AR-stage issues processing GF - specifically because if I have a really lovely thick coating of gold on an item it might not be affected by the nitric boils, and causes lots of problems because I have very dirty AR.
If you get too low the Gold will be in powder form and hard to separate.
At 25% it will form pieces that are easy to separate from the liquid.
 
Hi, thanks for the help.
The last nitric boil (pre-treatment) for my gold filled remained un-colored. I poured the solution into a large beaker where I have sterling to consume the nitric acid before putting into my waste stream.
I think my excess nitric was because I didn't pour off all that solution because I wanted to retain the colloidal gold I observed in the bottom. It didn't seem like that much but when I added HCL I didn't need any additional nitric to dissolve the gold. At this point, I surmised that I was at risk for having excess nitric but I've dealt with it before.
I filtered after the AR step till the solution was clarified but the color was very green-brown, as I said. Stannous test was, of course, positive.
New update - I shared my issue with chatgpt and it shared a few possibilities. One that stood out was this:

Iron Compounds: Since some of your jewelry is magnetic, it indicates the presence of iron. Iron can form various oxides and hydroxides that can appear black. When exposed to nitric acid and aqua regia, iron may form black iron oxide (Fe3O4) or hydrated iron oxide (FeO(OH)), which can precipitate and coat the copper.

I prompted chatgpt to give me a treatment for this and got a lengthy (but basically simple) treatment centered around ammonia. I checked Hoke's book and verified that it should work. I'll divide a small amount of the solution for experimentation and report the results.
Hi, could you share you way to get gold in this case,
I really want to know it because I got the same issue,
thank you,
 
If you can't find anything about Gold filled you need to improve your searches.
There are a lot of discussions on this topic.

But the general rule with Gold filled as anything mixed metal is:
Dissolve all the base metals first, then dissolve the Gold.

You have not yet detailed your process, but my guess is too much Nitric.

Cement it on Copper (with agitation) and redissolve the dropped powder for a cleaner drop.
Yggdrasil.. before you drop it you can't see many out first of copper and then drop gold after you clean the copper out...I was told once you drop Cooper you cannot get it gold
 
Yggdrasil.. before you drop it you can't see many out first of copper and then drop gold after you clean the copper out...I was told once you drop Cooper you cannot get it gold
I have trouble understanding your text so I answer as I believe you meant it.
You can't drop Copper unless you Cement it with a metal like Iron or Zinc.
Or very high concentrations of SMB and then the Gold is out a long time ago.
No problem dropping Gold unless the pH is too high.
 
Yggdrasil.. before you drop it you can't see many out first of copper and then drop gold after you clean the copper out...I was told once you drop Cooper you cannot get it gold
A more simple approach.

SMB or other precipitants do not drop Copper, at least not much under normal circumstances.

If you cement out the Copper with Iron or Zinc, Gold will come out at the same time.
On the other hand, if you cement with Copper, only precious metals and Mercury(if present) can come out.
 
I was told once you drop Cooper you cannot get it gold
Where did you hear that? it will be more like: once you drop you copper, the gold will follow. Always. (edited to say): should you somehow selectively have dropped you copper first. I think the gold will cement out simultaneously as there will be copper in solution. so the gold will come out "first" as the cemented copper dissolves when it displaces gold.
 