So I went in today and picked up 41g of gold filled lockets. After stripping out the trash I found one that wasnt marked as I would expect for gold filled. It looks like its marked AA 585 is a marking that im not aware of or did I just have a very lucky day?

20180323_103131.jpg

20180323_103109-0.jpg
 
Thats what I figured but didnt know about the AA before the 585. Guess I need to run back in and talk to the owner of the shop.
 
I dont have anything with me at the moment, but ill grab a file and put a drop of nitric on it to see. It weighed in at 3.8g so if its 14k I owe a lil more than the .80 cents a gram I paid.
 
You wouldn't believe how much karat can find it's way into GF.
Most karat mixed with GF usually won't have any markings at all.
 
Palladium said:
You wouldn't believe how much karat can find it's way into GF.
Most karat mixed with GF usually won't have any markings at all.

I picked up 151 grams of GF last night and got one 12k gold ear ring, a tiny one at that. Out of 123 grams I got in today, I just took out a pair of cuff links marked 10K. I have already made good on the large lot to cover the plated items instead of returning the ear ring. The small lot was from several sources and I have no way of knowing who the cuff links actually came from. Those two finds seemed really odd, but on the previous two lots I found several items unmarked and ran them separate, the 4 pieces alone returned .3 grams of clean gold. Sometimes curiosity don't kill the cat, :D
 
Do you buy the filled gold pieces from Jewelers? Is it common for them to sell it?

Sent from my LG-H872 using Tapatalk
 
rickzeien said:
Do you buy the filled gold pieces from Jewelers? Is it common for them to sell it?

Sent from my LG-H872 using Tapatalk

Most of mine come from yard sales, flea markets and certain kinds of thrift stores. I do buy some from a gold buyer, but I also process some for him as well. I have known most of my sources for many years, just from working with them in other areas. Much of my computer scrap came from the shop where I bought my computers for years. The thrift shop type I look for are the small ones, what I term "Mom and Pop" type shops. Again I buy gold filled at a couple of them. And again, they were people I have known for a very long time. I also spent some time convincing them to buy it, as their normal gold buyer doesn't. One of my main sources is a coin dealer that I have known since the early 1990's that also buys gold and silver. Since I have been working his gold filled for him, he has started questioning me about doing some of his silver as well. Soon as I have this next lot ready, we will be discussing that as well.

Some of my advice, become a bit OCD about it, talk to everyone all the time looking for sources, while being a bit cautious as well. Some good sources come from some rather odd places.
 
Shark said:
rickzeien said:
Do you buy the filled gold pieces from Jewelers? Is it common for them to sell it?

Sent from my LG-H872 using Tapatalk

Most of mine come from yard sales, flea markets and certain kinds of thrift stores. I do buy some from a gold buyer, but I also process some for him as well. I have known most of my sources for many years, just from working with them in other areas. Much of my computer scrap came from the shop where I bought my computers for years. The thrift shop type I look for are the small ones, what I term "Mom and Pop" type shops. Again I buy gold filled at a couple of them. And again, they were people I have known for a very long time. I also spent some time convincing them to buy it, as their normal gold buyer doesn't. One of my main sources is a coin dealer that I have known since the early 1990's that also buys gold and silver. Since I have been working his gold filled for him, he has started questioning me about doing some of his silver as well. Soon as I have this next lot ready, we will be discussing that as well.

Some of my advice, become a bit OCD about it, talk to everyone all the time looking for sources, while being a bit cautious as well. Some good sources come from some rather odd places.
Thank you for the advice.

Sent from my LG-H872 using Tapatalk
 
All my gold filled comes from a jewelry/coin store not that far from me. They are one a a small handful of ahops that are willing to sell. I have only done small test batches to get the process down so far but as soon as my nitric gets here I have half a pound waiting. Maybe there will be more surprises in the pile. I sorted it out tonight and found about 85g of unmarked chains in the pile.
 
I never look for karat in the first step. After a nitric wash to remove the base metals any karat mixed in will be easily identified and removed. Most times i just carry in on over to ar. If there is anything left after that what is left will show up as a crusted piece in the final filter residues.
 