I am doing my first Au refine from gold fingers. I haven't gotten far and I'm already confused... I have 250g of fingers in 730ml of 10% HCl. I boiled for about 20 minutes and the small amounts of solder that were present dissolved but some of the fingers turned a dark grey color. Others have changed color a little. I have attached a before and after picture of one of the pieces. What would cause this?
Also, on a related note, can someone point me to a tutorial thread here for this process? I had planned to use HCl to remove the solder, nitric to liberate the foils and then aqua regia to dissolve them, sulfamic acid denox and SMB precipitation.
Thank you!
Eric
Also, on a related note, can someone point me to a tutorial thread here for this process? I had planned to use HCl to remove the solder, nitric to liberate the foils and then aqua regia to dissolve them, sulfamic acid denox and SMB precipitation.
Thank you!
Eric