Hello, I am about two months into Gold Refining and I have realized that this is NOT as easy as it looks.
Here is my dilemma:
I separated my gold into a pile of gold plated circuit boards with a whole lot of other components soldered in place. There was no practical way to isolate just the gold areas. I then started the Acid Peroxide (AP) process. The AP process went exceptionally well - causing the gold foil/flakes to float in the AP solution.
I then filtered as much "gunk" out as I could, and then I proceeded with the Aqua Regia (AR) process. This left me with a “goldish colored” solution. A stannous test showed an instant dark brown stain (but no purple). Home free, right? Wrong.
I denoxed it with urea and I could not drop any gold out with the addition of SMB. I then tried a little sulfamic acid and the same result – NO gold drop. Are the other dissolved metals causing mayhem?
Any thoughts would be appreciated?
Here is my dilemma:
I separated my gold into a pile of gold plated circuit boards with a whole lot of other components soldered in place. There was no practical way to isolate just the gold areas. I then started the Acid Peroxide (AP) process. The AP process went exceptionally well - causing the gold foil/flakes to float in the AP solution.
I then filtered as much "gunk" out as I could, and then I proceeded with the Aqua Regia (AR) process. This left me with a “goldish colored” solution. A stannous test showed an instant dark brown stain (but no purple). Home free, right? Wrong.
I denoxed it with urea and I could not drop any gold out with the addition of SMB. I then tried a little sulfamic acid and the same result – NO gold drop. Are the other dissolved metals causing mayhem?
Any thoughts would be appreciated?