Help with next steps.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Joined
Nov 22, 2024
Messages
6
Hello everyone! This is an amazing community with lots of knowledge and I appreciate being able to join the group. My husband started the refining process on some ore he gathered. This is 3:1 Hydrochloric Acid and Nitric acid mixed with the crushed ore. He's not exactly sure where to go next with it so I thought I would reach out to gather more knowledge. Thank you all for any help in advance.
1000001181.jpg
 
Hello everyone! This is an amazing community with lots of knowledge and I appreciate being able to join the group. My husband started the refining process on some ore he gathered. This is 3:1 Hydrochloric Acid and Nitric acid mixed with the crushed ore. He's not exactly sure where to go next with it so I thought I would reach out to gather more knowledge. Thank you all for any help in advance.
View attachment 65931
Welcome to us.
He has already started out in the wrong end.
One simply do not use Aqua Regia on ores.
Way too dangerous, expensive and creating too much waste.
Do you have an Assay.
Or Stannous chloride to test with?
 
Welcome to us.
He has already started out in the wrong end.
One simply do not use Aqua Regia on ores.
Way too dangerous, expensive and creating too much waste.
Do you have an Assay.
Or Stannous chloride to test with?

Welcome to us.
He has already started out in the wrong end.
One simply do not use Aqua Regia on ores.
Way too dangerous, expensive and creating too much waste.
Do you have an Assay.
Or Stannous chloride to test with?
No on both but I found stannous chloride to test with online that I can purchase. Do you have a preference? We do have a list of what is in the ore. Thank you for your time and information.
 
No on both but I found stannous chloride to test with online that I can purchase. Do you have a preference? We do have a list of what is in the ore. Thank you for your time and information.
No need to buy Stannous, just dissolve some Tin Solder in HCl.
So how do you know what is in the ore if you have no assay?
 
An assay tests the ore and lists what is in it.
Such as good things and bad things and it will to some degree decide how you treat it.
Edit for spelling
 
Last edited:
How was it processed then?
And what do that list show?
I can't find how it was processed. I have also made him very aware of the dangers of arsenic. I read the information posted on here a few days ago. Is smelting better with the arsenic than aqua regia? I'm attempting gain as much information as possible. Thank you!
 

Attachments

  • IMG_20241124_152151.jpg
    IMG_20241124_152151.jpg
    225.4 KB
I can't find how it was processed. I have also made him very aware of the dangers of arsenic. I read the information posted on here a few days ago. Is smelting better with the arsenic than aqua regia? I'm attempting gain as much information as possible. Thank you!
That was what I was afraid of.
Dissolving Arsenic has made it much more dangerous.
Set this lot aside in closed containers.
Take a trip to a doctor for a checkout and tell what has been done.
For proessing I guess it all depends on the form the Gold have in the ore.
In the old days it was probably crushed and gravity separated.
 
Ok. It's been a few months since the did it. The rest of us weren't home and haven't touched it. Would smelting it be better?
I'm not sure when it comes to Arsenic.
The best is if the Gold can be separated without heat or chemicals I guess.
 

Latest posts