There are many recipes out there, but why make our simplest task difficult.
Fill a 50-100ml bottle with a splash (a few ml) water add HCl to 3/4 full and put in a few grams of Tin solder.
Let it react until the bubbles stop.
Add a cap loosely.
It is beneficial that not all the Tin dissolves if you want it to keep working for a long time.
For your own sake it is wise to write down your own recipe so you make the same strength each time.
Thanks! It was so simple, I couldn't understand it.
 
Working on stannous chloride .
Gold testing solution next.
Litmus paper strips ordered instead of pH meter
 

Attachments

  • EBF15038-4DAE-4198-8D8E-86A1E502662F.jpeg
    EBF15038-4DAE-4198-8D8E-86A1E502662F.jpeg
    2.8 MB · Views: 0
Ok so I was going to run/ process another batch of foils and 1/20 14-10K gold filled jewelry .
Here are the steps I was going to use.
Soak in AP
filter
HCl + Bleach ( cold )
Filter
Drop w/ SMB.
 
Ok so I was going to run/ process another batch of foils and 1/20 14-10K gold filled jewelry .
Here are the steps I was going to use.
Soak in AP
filter
HCl + Bleach ( cold )
Filter
Drop w/ SMB.
The thick foils from Gold filled may not dissolve easily in HCl/Bleach.
Better with AR or at least HCl/ pool-Chlorine or strong Peroxide.
 