Ok so I ran a few batches of gold filled, burned and processed my filters I have built up and processed nitric waste i been pouring over some gold colored chalices mark international silver co. in a collection pot and processed the other stock pots for any waste. Did several nitric dissolutions on all that for a single AR. I didn't get any silver out from the nitric solution even after a day of leaving copper in to cement. So ok I took all the filtration from the batches and filters and incinerated then into AR. Filtered solution added ice and sodium metabisulfite to percipitate the gold. I knew some gold was in solution from a stannous test. After a few hours or so I looked at it and these crystal formation are dropping out. (See photo) does anyone know what is dropping out so I know what to do with it? I.e. run thru nitric again to seperate and then thru AR to get gold out. Or if this is something other then silver or gold. I wouldn't think it's silver cause silver would have come out at the nitric phase of dissolution. I've just never had this reaction with metabisulfite to percipitate gold before.