Has anyone ever run this type of material.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

escrap

Well-known member
Joined
Oct 23, 2009
Messages
195
We have close to 250lbs of this material that we got out of a warehouse clean out. The other material that was with it was dated mid-late 70's. From the looks of it, the material seems to be pretty nice. But I wanted to see if anyone knows how good it may be. I have cleaned 5 lbs and got 1.5lbs of cleaned material. Thanks in advance for the advice.
 

Attachments

  • 20121009_150104.jpg
    20121009_150104.jpg
    2.4 MB
  • 20121009_150046.jpg
    20121009_150046.jpg
    2 MB
  • 20121009_150113.jpg
    20121009_150113.jpg
    2.4 MB
what are the dimensions? they look to be about 0.30USD apiece in gold.

1 sq inch @ 30 micro inches is 0.54USD today with gold @1762.00USD
http://goldnscrap.com/index.php?option=com_content&view=article&id=72:gold-plating-calculator&catid=49:calculators&Itemid=66


if you take them off the white part leave the wires on you might be able to run the real easy in a cell by conesting the wires at the end.


Eric
 
ive ran many of them. they do yield high, well more than computer pins. on average about .4g per US pound maybe a little better.

this was almost two years ago and my memory may be faulty.after thinking about it, i may have gotten things backwards, instead of 2.5 pounds per gram, it may have been 2.5g per pound. if it is, im sorry to have mislead anyone.
 