I apologize, I'm sure the information I want is here somewhere I just can't seem to find it searching or in the library.

What is the process for dissolving gold foils (from AP-digested fingers) using HCl and bleach? I am thinking of submerging the foils in full-strength HCl and then adding small amounts of bleach, step-wise until they are gone. I assume room temperature/cold is better for keeping the Cl in solution? Don't add too much bleach at once so Cl doesn't blow off? I saw someone say that the bleach should be injected at the bottom of the mixture, though I'm not sure why.

Once dissolved and filtered, I have SMB for reduction. Is any post-processing of the resulting mixture needed before SMB?

Any specific advice would be appreciated, thank you!
 

Attachments

  • IMG_0295.JPEG
    IMG_0295.JPEG
    980.3 KB
Last edited:
I apologize, I'm sure the information I want is here somewhere I just can't seem to find it searching or in the library.

What is the process for dissolving gold foils (from AP-digested fingers) using HCl and bleach? I am thinking of submerging the foils in full-strength HCl and then adding small amounts of bleach, step-wise until they are gone. I assume room temperature/cold is better for keeping the Cl in solution? Don't add too much bleach at once so Cl doesn't blow off? I saw someone say that the bleach should be injected at the bottom of the mixture, though I'm not sure why.

Once dissolved and filtered, I have SMB for reduction. Is any post-processing of the resulting mixture needed before SMB?

Any specific advice would be appreciated, thank you!
Your plan will work.
The not add too much bleach goes equally much into not neutralizing the HCl.
Nothing special to do after dissolving, just let it sit a day or so or give it a good heating, not boil.
 
@eprigge Just to add that the solution needs to be stirred a lot while adding the bleach, as the chlorine gas produced needs to make actual contact with each of the gold foils in order to dissolve them. I'm guessing that's the reasoning for the suggestion of injecting it at the bottom of the solution but stirring should work fine.
Yes room temperature is best as heat will drive off the chlorine too quickly and you'll just need to use more bleach than necessary.
Also consider how chlorine gas can be removed from the workspace, if you don't have a fume hood do it outside and stand upwind- or better if you can rig up a fan with some ducting it will make the job less unpleasant.
 
Last edited:
Thanks guys. Yes, I see what you mean regarding solubility vs temperature. Diluting the HCl with water (having more solution) would help to keep the Cl from outgassing. Unless the pH has to be at a certain level. I have 20 deg Baume HCl so I could dilute it by over 8x and it would have a pH of zero. I know the bleach will consume acid. I'll cut the acid to 25% strength and use a larger volume of it. And use a stirrer at 40-50 F. At this temp, the solution should hold 10g Cl/L.
 