Hi together!!
I'm from Malaysia and this is my first post since i have read a lot of
valueable information here.Thanks to lazersteve video and members here.
This is my first experiment:
Method: AP
Acid:Hydroklorik 37% , Peroxide 3% and clorox 5.25% sodium hypochlorite
600g trimmed fingers from HP Server Board
filled in a drill hole bucket like steve video,
The drill bucket put in a large bucket
Then i put 2 liter HCL and 1 liter Peroxide
The foils stripped nicely after 4-5 days..
Wash foils for several rinse with HCL and Hot Water
What is happen here, when i process foils with HCL/CL,it turn to light/ green,green color.
Its look like im stuck here,So i save the solution in safety place for later process.
I do not have Stannous on hand,because hard to find in my area.
Any advice would be great and thanks again.
Izam
I'm from Malaysia and this is my first post since i have read a lot of
valueable information here.Thanks to lazersteve video and members here.
This is my first experiment:
Method: AP
Acid:Hydroklorik 37% , Peroxide 3% and clorox 5.25% sodium hypochlorite
600g trimmed fingers from HP Server Board
filled in a drill hole bucket like steve video,
The drill bucket put in a large bucket
Then i put 2 liter HCL and 1 liter Peroxide
The foils stripped nicely after 4-5 days..
Wash foils for several rinse with HCL and Hot Water
What is happen here, when i process foils with HCL/CL,it turn to light/ green,green color.
Its look like im stuck here,So i save the solution in safety place for later process.
I do not have Stannous on hand,because hard to find in my area.
Any advice would be great and thanks again.
Izam