Man. Is that a unlimited supply?I have never liked saying prices, but I have been paying $9-$10 per pound for mixed ram for several years. Note I said mixed. I can refine at this price and make a little or I can sort and resell and still make a little from it. To be fair check the pricing on places like Boardsort or other similar sites to get a better idea. Just guessing, but I am thinking around $25 to $30 pound being the average going rate they pay and that won't leave much room to make a profit at all. Compare their prices and adjust according to your ability to refine or have margin room to resell at a small profit.
And what do you think will it cost to buy all the equipment for recovering the gold from the ram? And what tools are really necessary? Best Regards, DevastatorI have never liked saying prices, but I have been paying $9-$10 per pound for mixed ram for several years. Note I said mixed. I can refine at this price and make a little or I can sort and resell and still make a little from it. To be fair check the pricing on places like Boardsort or other similar sites to get a better idea. Just guessing, but I am thinking around $25 to $30 pound being the average going rate they pay and that won't leave much room to make a profit at all. Compare their prices and adjust according to your ability to refine or have margin room to resell at a small profit.
To be honest I haven't bought much equipment in several years. I bought the majority of what I need back when I started. I would study some, as you learn the varying processes you gain an understanding of what you need as well.And what do you think will it cost to buy all the equipment for recovering the gold from the ram? And what tools are really necessary? Best Regards, Devastator
I wish I had an unlimited supply of ram cards at that price. I'd purchase a ton of them...literally.No it's not unlimited, just a price the seller is happy with and I am happy with.
I had a similar question and I am figuring it out.Hi, I want to get into gold recovery and don‘t really know the value of e-scrap. I have the chance to buy some Ram, so I wanted to ask how much you guys would be willing to pay for 11.5 kg of ram, or how much you think it is worth. Please let me know
I have never seen yields on these.Heey guys instead of RAM fingers how about TV/Monitors boards. How much would a kilo of this yield?? Just the gold fingers, excluding the IC's? I would be blessed with your data and knowledge. Thank you have a Good day.
View attachment 65338View attachment 65337
Okay, Maybe I'll find out. It's cheap to buy this scrap but it only contains 1 or 2 IC chips. I'll try this experiment and find what value and yields I'll get.I have never seen yields on these.
But my guess is that the majority of the values are in the Chips/ICs
Generally speaking, if something is cheap it has little value.Okay, Maybe I'll find out. It's cheap to buy this scrap but it only contains 1 or 2 IC chips. I'll try this experiment and find what value and yields I'll get.
Those are fetching $10k per tonne so they aren't as bad as they look. TV/monitor screen strips.Generally speaking, if something is cheap it has little value.
That may hold true here or maybe not.
So approximate 10 a kilo then, not too bad.Those are fetching $10k per tonne so they aren't as bad as they look. TV/monitor screen strips.
Those are fetching $10k per tonne so they aren't as bad as they look. TV/monitor screen strips.
$10000 | 1000 kg |
$1000 | 100 kg |
$100 | 10 kg |
$10 | 1 kg |