How much soduim metabisulfite to drop gold.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
1 gram of smb for every gram of gold you expect usually, sometimes a bit more. This is being discussed currently in another thread, and is all over the forum. It would help others if people would use the search function or read a bit before asking questions. Pretty please :D
 