• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

How to build a stripping cell

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

alb320

Active member
Joined
Mar 31, 2008
Messages
40
Location
Italy
Hi guys..
I would have some advices for build a stripping cell.
I'm going to use it for deplate 6kg/8kg of gold plated items..
What power supply I have to use? How much of Volt, Amp?
And... what material I could use for build anode and cathode?

Looking for your advices...
 
Since thay are all watch cases, and roughly the same size, why couldn't a guy just hang them in a row by copper wire from a stainless or copper rod as the anode.
Have an oblong rectangular lead bar or strip as the cathode, and just lower them in manually, turning the rod of parts around when one side is stripped.
If this is a one time thing the labor involved might not be too bad.
Do something like 10 at a time, or more.........
Just an idea......
 
Platdigger.. thank for your advice, but I would buil a cell to use with other items, also.
Have you some experience with reverse cell? or with stripping cell?
 
Lasersteve has a very good vidio that explains and shows the process.

http://www.goldrecovery.us/index.asp

Go to the above link and follow the directions to reverse plating. It will answer most of your questions.

Good luck

Emil
 