I cant sling pins for the life of me, so instead, try this. Heat up the BBQ grill ( the one you dont use for food) set a few fire bricks in it and let them heat up too. when it gets to 400+ set your fiber CPU's on the bricks the one's with the kovar pins (legs), let them come up to temp. Then hold a Hard drive magnet above the pins, use a non magnetic rod to keep the chip from moving. Bingo, all the legs jump up to the magnet, and nothing is lost due to poor technique, and the chips dont burn.