The mine slime content is as follow
gold ~2000ppm
silver ~7000ppm
platnium ~4ppm
palladium ~10ppm
nickel ~2%
copper ~27%
selenium ~7%
arsenic ~1000ppm
chloride ~1000pm
i know that arsenic is a very strong posion to human and environment
1.) so is 1000ppm of arsenic dangerous?
2.) how to remove the arsenic without losing the metal content?
3.) how to extract and refine the selenium?