I hope this post finds everyone making .9999
I am trying to find the answer as to how cemented COPPER should be stored (after drying) or stored under a liquid until smelting?
I got most of my gold out of solution based on my calculations cementing on copper. Now I have started that solution cementing out copper onto iron/steel. I placed the bar stock only half under the solution.
This was after 24 hours with a bubbler going:
From the looks of it, this is either silver or tin. I guess my solution was not as "barren" as I thought. The newest layer looks almost entirely like copper.
Should I dry it out, or keep it under water?
My goal is to make my own Cu rounds.
This is just for reference
I am trying to find the answer as to how cemented COPPER should be stored (after drying) or stored under a liquid until smelting?
I got most of my gold out of solution based on my calculations cementing on copper. Now I have started that solution cementing out copper onto iron/steel. I placed the bar stock only half under the solution.
This was after 24 hours with a bubbler going:
From the looks of it, this is either silver or tin. I guess my solution was not as "barren" as I thought. The newest layer looks almost entirely like copper.
Should I dry it out, or keep it under water?
My goal is to make my own Cu rounds.
This is just for reference