I over shot my nitric so I cooked the AR down to a solid and added more HCL but it's still full of salt. What should I do next?
Of course it is full if salts, they usually do not evaporate.I over shot my nitric so I cooked the AR down to a solid and added more HCL but it's still full of salt. What should I do next?
Of course it is full if salts, they usually do not evaporate.
But there should not be any mote Nitrates and Nitric left.
So what is your plan with the salts?
Drop the Gold?
Then add HCl until it is all dissolved and then drop it with your preferred me
You should be able to dissolve most, then filter what is left and drop.So just filter the salts? Then drop?
Was it positive before evaporating?Should I just re-dissolve everything (using tiny amounts of nitric this time) then precipitate?
Then it may have decomposed to metal.Yes! Very much so
In the case of Bleach there is no need for driving off the NitricBleach is better? In this case?
AR solution is full of soluble chlorides, that do not evaporate. And as it is already completely saturated with chlorides, putting HCL (fairly concentrated chloride - 10+ molar by the way) will do what is expected - rise the chloride content and crash out the chlorides as precipitates - as they cannot be dissolved anymore.I over shot my nitric so I cooked the AR down to a solid and added more HCL but it's still full of salt. What should I do next?