Hi guys,
This is the way of my "gold mining" from ic's.
Sorry for my English, i'm from Slovakia, very nice country .
All I need is a drill, bearing balls, steel container and old pulley. Bearing balls are mixed with ic's in steel container. Then just turn on the drill with the pulley. The process takes about 10 minutes (cca 250g of ic's). Then just wash the impurities and gold settle to the bottom. And result is very beautiful, 0.5g of gold wires.
Thank you all, for the inspiration on the forum.
This is the way of my "gold mining" from ic's.
Sorry for my English, i'm from Slovakia, very nice country .
All I need is a drill, bearing balls, steel container and old pulley. Bearing balls are mixed with ic's in steel container. Then just turn on the drill with the pulley. The process takes about 10 minutes (cca 250g of ic's). Then just wash the impurities and gold settle to the bottom. And result is very beautiful, 0.5g of gold wires.
Thank you all, for the inspiration on the forum.