hello everyone-again,
i've made some littles test in the past with different material but everytime it was a gold plated metal part firmly connected with its plastic casing...or high quantities so a hand out pulling is an absolute no go.
there was different metals and different plastics but every time after the incineration i'am not able to see the gold plating on the freed metal parts...only the base metal.
i didn't through the objects in a hellfire, i incinerate them very carefully and as "cold" as possible with an reducing flame....an as slow as possible....no glowing of the metal parts.....
i am not shure if the aggressive fumes of the burning plastic made something with the gold (i know...not realistic) ot if the gold diffused into the metal and so it isn't longer vissible?
is there anybody who share my observations or, much better, somebody who is able to explain what there happens?
best regards, frank!
i've made some littles test in the past with different material but everytime it was a gold plated metal part firmly connected with its plastic casing...or high quantities so a hand out pulling is an absolute no go.
there was different metals and different plastics but every time after the incineration i'am not able to see the gold plating on the freed metal parts...only the base metal.
i didn't through the objects in a hellfire, i incinerate them very carefully and as "cold" as possible with an reducing flame....an as slow as possible....no glowing of the metal parts.....
i am not shure if the aggressive fumes of the burning plastic made something with the gold (i know...not realistic) ot if the gold diffused into the metal and so it isn't longer vissible?
is there anybody who share my observations or, much better, somebody who is able to explain what there happens?
best regards, frank!