Electrochemistry Interesting idea in an old thread- dissolving gold in a Chlor-alkali cell

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Depending on the conditions, Gold seem to precipitate between 4.5 to 13 pH.
So this is at least not suited for separation this way.
But since you already are planning a pump, maybe pump it past a Copper system to Cement the Gold in circuit?
Maybe indeed.

There's also the issue of hydrogen production to consider...
 