Is it possible To...?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

kjavanb123

Well-known member
Joined
Apr 1, 2009
Messages
1,746
Location
USA
Hi

i am really confused here, is it possible same tailing sample get litterly the same results when sent to assaying labs, yet using fire assayit gets different result?
 
My opinion only.

Trust a fire assay. If it fire assays, it will produce.

That's assuming your assayer isn't crooked, or unskilled.

Never lose sight of the possibility that you are being taken for a ride. Crooks work in strange and mysterious ways. Shysters have been working hard on "prospectors" for years, many with claims of "immature" gold, which won't fire assay, but is present, detected by other methods.

Anyone that can believe that deserves to lose. Gold is an element. It is gold, or it isn't. I know of nothing in between.

Harold
 
There are some complex sulfide ore's that produce more gold when leached, than the fire assay said it should have contained.

Now on the other hand, if your other assays are producing less than the fire assay results, then there is probably someone trying to rip you off.

Mark
 