I answered your question several times, I said I naturalize the chemical waste with NaOH after precipitating copper by iron as a final step.You keep ignoring or dodging the question: How do you process your wastes?
No, this is the first time you mention cementing on Copper and Iron.I answered your question several times, I said I naturalize the chemical waste with NaOH after precipitating copper by iron as a final step.
Yes, I just mentioned NaOh, but I was mean after getting copper, who left copper behind!No, this is the first time you mention cementing on Copper and Iron.
But if you follow the instructions in dealing with waste you should be good.