Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.
They're not cheap.
https://encrypted.google.com/search?hl=&q=induction+furnace+platinum&sourceid=navclient-ff&rlz=1B3MOZA_enUS408US409&ie=UTF-8&aq=0&oq=induction+furnace+plat&lr=all
Amalgamite is the name I've heard associated with bismuth. So platinum dissolved into molten bismuth, sort of deceptive in that it's not hot enough to melt pure platinum and you end up with an alloy button.
well i melted platinum with gloor torch and propane-butan/medical oxygen gas,
the platinum was in powdered form and it melted perfectly, i even tried to remelt it and I was successful.
It was done on chamotte brick.
It is possible to melt it with propane...
Due to large surface in powdered form(black powder) m.p. is very low , around 900 celsius.
In very small spheres platinum is also possible to melt with propane, if the torch diameter is bigger then diameter of spheres.But the mixture of prop-bu/O2 must be at maximum
pressure. available on exit from the torch- max throttle...
Kats