Pulled this from a newer microwave, in my head it would be goldplate to help in shielding, but I guess this could just be brass.
Ok thank you!I'm going to go with Brass Famagus.
Pulled this from a newer microwave, in my head it would be goldplate to help in shielding, but I guess this could just be brass.
This one is only a couple years old it was dropped and the door broke. Unfortunately a replacement door wasn't far off from the cost of a new microwave so I decided to see what all it had.Careful with those magnetrons, I hear some of the older ones may contain Beryllium.
We do not delete posts here, unless it is scamming, spamming or profanities.I had just found a post regarding this exact topic! So I guess I should delete this post as it's already been covered!
Ok good to know!We do not delete posts here, unless it is scamming, spamming or profanities.
Picture number two in the orginal post show the pink berylium porcelain, it is in the middle of the gold looking brase ring.Careful with those magnetrons, I hear some of the older ones may contain Beryllium.
I'll make sure not to damage it and set it all aside till I have a reliable buyer that will take it off my hands! Thank you for identifying it for me!Picture number two in the orginal post show the pink berylium porcelain, it is in the middle of the gold looking brase ring.
It is the dust there is very dangerous, so dont breake it. If you have enough you can sell it for a good price. Please notise you have to make sure the berylium dosent harm anybody in the future.
In the good old days there was a cobber coil about 10 pound/4 kg (6$ worth where i live) now they mostly made by copper plated alu wire.
Henrik
Careful with those magnetrons, I hear some of the older ones may contain Beryllium.
It is the dust there is very dangerous, so dont breake it.