Need to run some number's by you guys. My yields from cpu’s seen a little low?
1. Pen Pro .25 g
2. Pen Reg .07g
Are the numbers right
I did 2 pen pro’s and got ½ g Then I did 4 pen pro’s and got 1 g the number’s work out…
I’m using the poormans AR system…getting great gold at the end but not as much as I should.
there no way im losing gold by leting the solution evaporate down to 25% of it's original volume, or until salts form
Help
1. Pen Pro .25 g
2. Pen Reg .07g
Are the numbers right
I did 2 pen pro’s and got ½ g Then I did 4 pen pro’s and got 1 g the number’s work out…
I’m using the poormans AR system…getting great gold at the end but not as much as I should.
there no way im losing gold by leting the solution evaporate down to 25% of it's original volume, or until salts form
Help