gold ~3 mils on foil, 4 inches x 36 - 40 inches , weight 4+ grams, one side shiny gold, other side dull gold, some small unplated spots, many availablegold foil 2024.jpg
 
Dutch metal is a form of brass. The alloy typically consists of 85–88% copper and the remainder being zinc. It is also known by other names such as "composition gold leaf", "Dutch gold", "Schlagmetal" and "Schlag leaf".[1]

It is very malleable and ductile and so can be beaten into very thin sheets. These sheets are sold for use as metal leaf or imitation gold leaf.[2] The addition of arsenic produces an alloy with similar properties but coloured white
:)
 