I first was on the impression that this was plastic, as this was the body of the pen from an old digitizer.
When i then pick the parts apart i accidently droped it on a wooden floor, and the sound it gave when it hit the floor took me by surprise.
It sounded like an instrument, almost like a tuningfork.
It was coated with a really thick layer paint, and under is a shiny white metal.
I tried heating it and it became maleable when heated with a butan torch , the paint took the fire like a champ , ( yes i use ppe ).
Not magnetic, Have not tried paramagnetism yet, i think i will.
I have a clue what tis could be, but i am real curiuos what you experts think.

Best regards to all of you / Arne
 

Attachments

  • IMG_20240904_221747.jpg
    IMG_20240904_221747.jpg
    2.3 MB
  • IMG_20240904_221747.jpg
    IMG_20240904_221747.jpg
    2.3 MB
  • IMG_20240904_221757.jpg
    IMG_20240904_221757.jpg
    2.3 MB
  • IMG_20240904_221815.jpg
    IMG_20240904_221815.jpg
    874.8 KB
I first was on the impression that this was plastic, as this was the body of the pen from an old digitizer.
When i then pick the parts apart i accidently droped it on a wooden floor, and the sound it gave when it hit the floor took me by surprise.
It sounded like an instrument, almost like a tuningfork.
It was coated with a really thick layer paint, and under is a shiny white metal.
I tried heating it and it became maleable when heated with a butan torch , the paint took the fire like a champ , ( yes i use ppe ).
Not magnetic, Have not tried paramagnetism yet, i think i will.
I have a clue what tis could be, but i am real curiuos what you experts think.

Best regards to all of you / Arne
In the pictures it look like Copper.
 
Last edited:
need weight.
similar to nickel silver, an alloy of nickel, zinc and copper... with a high nickel content.
maybe that’s why it’s painted over, many people are allergic to nickel
 