jacknicholson
New member
- Joined
- Aug 1, 2011
- Messages
- 2
Can't get to the video link, it seems to be broken. Is the video posted anywhere else?
Thanks,
Thanks,
Dude4ever said:How do you know that chlorine is out of solution and that it is safe to drop with SMB?
goldscraphobby said:I never heat, I use a strong bottle (usually a cleaned simply orange bottle) add the gold & HCl, then I put in the chlorine and close it tight. Shake it up and let it sit. Every once and awhile shake it real good to mix it around. Not in a rush so I let it take its time.
Just don't put too much to exceed the pressure of the bottle. Never had an issue and reduces the amount needed.
saadat68 said:Hi
If I want dissolve some gold powders or gold foiles with hcl/cl method but without heating solution
How much time I must wait between adding shots
(I know with heating we must wait 1 to 5 minutes and then add another shot of chlorex)
Thanks
anachronism said:saadat68 said:Hi
If I want dissolve some gold powders or gold foiles with hcl/cl method but without heating solution
How much time I must wait between adding shots
(I know with heating we must wait 1 to 5 minutes and then add another shot of chlorex)
Thanks
The simple answer is "until it not doing anything."