geubrina said:My friend told me that adding some Sodium Nitrate and Ammonium Chloride together with Borax, will improve the melting of gold powder performance.
I want to try but here, the smallest batch to buy sodium nitrate is 500 kg.
Platdigger said:I think you could make it from ammonia nitrate or calcium nitrate, if you had one of those.
But not sure how....Irons???
Randy
Irons said:Platdigger said:I think you could make it from ammonia nitrate or calcium nitrate, if you had one of those.
But not sure how....Irons???
Randy
Add Sodium Hydroxide for the NH4NO3 and Sodium Sulfate for the Calcium Nitrate,
First get the Gold from the ore and start from there.
Since we don't know what the ore is, it's difficult to give advice.