Hi, after i took out the silver from my solution, how do i get metalic copper from it, i refined gold by this method an it has lot of copper, thanks...
In the safety section if you read dealing with waste it will cover cementing the copper out with Iron, and how to treat the solution for waste, this topic and the safety thread is a must read for anyone serious about recover and refining of metals.