Yes.

The top one is pretty small. It will cast bars about 4 1/2" long and about the diameter of a nickle.

The bottom one is a piece of angle cut from a bed rail and can be poured thinner or thicker to suit the need.
 
Rick,

Good use for that olivine might be to cast yourself some nice molds in cast iron.

I have about 3500 lbs of 60 mesh and if you had anything finer so I can diversify I would appreciate it!

Furnaces look awesome.
 
Lou said:
Rick,

Good use for that olivine might be to cast yourself some nice molds in cast iron.

I have about 3500 lbs of 60 mesh and if you had anything finer so I can diversify I would appreciate it!

Furnaces look awesome.
Not sure what mesh it is. I will check and get back to you.

Sent from my SM-G950U using Tapatalk

 
If you pour cast iron and mold your own molds, you will need to post some pictures/videos of that process as well....... :lol: :lol: :lol:
 