My first button 4.15 grams. Thanks for all the help everyone couldn't have done it without all the great information on this forum!!!! :lol:
 

Attachments

  • 20130927_150238.jpg
    20130927_150238.jpg
    2.6 MB
  • 20130927_150233.jpg
    20130927_150233.jpg
    2.1 MB
Thank you so much couldn't have done it without you samuel-A and the rest of the forum. I refined a few ceramics and followed the process that I read from your website. But that was just a small amount of what i did. I ran some fingers, pins, ceramics, and black fiber cpus to get this button. Just experimented with a few of the processes to try and get a feel for them and this is what I got. Thanks for the kind words. Feels good, I am definitely hooked!!
 
very nice button. nice color and shine. you can tell it cooled slowly because of the shape of the button. if it had been melted well, it would have more round.
 