S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 25, 2008 #1 I add sodium nitrate and Hcl enough.. all cpu dissolve and I have very dark green Ar solution I fileter it and add Smb And now my bottle down have crystal MASS.. it is maybe silver I dont know I will send pic
I add sodium nitrate and Hcl enough.. all cpu dissolve and I have very dark green Ar solution I fileter it and add Smb And now my bottle down have crystal MASS.. it is maybe silver I dont know I will send pic
S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 25, 2008 #2 what is that ??
P Platdigger Well-known member Supporting Member Joined Jul 26, 2007 Messages 1,662 Location Washington Oct 25, 2008 #3 Did you "kill" or eliminate the nitric before adding the smb? Randy
S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 25, 2008 #4 yes mate I killed with urea.. I add urea to not see fizz I am not sure SMB My chemicals seller have wrong.. he is write on pack smb but I am not sure.. I have 3 pack One is Smb one Borax other ammonium clorur if he have wrong maybe this ammonim clorur ? as for you this result norml with ammonium clorur ?
yes mate I killed with urea.. I add urea to not see fizz I am not sure SMB My chemicals seller have wrong.. he is write on pack smb but I am not sure.. I have 3 pack One is Smb one Borax other ammonium clorur if he have wrong maybe this ammonim clorur ? as for you this result norml with ammonium clorur ?
P Platdigger Well-known member Supporting Member Joined Jul 26, 2007 Messages 1,662 Location Washington Oct 25, 2008 #5 Did you disolve the smb in water before you added it? If so, did you get a wiff of the smb? You won't want to, trust me on that, but if you did, you could definitely distinguish it from the other chems. Randy
Did you disolve the smb in water before you added it? If so, did you get a wiff of the smb? You won't want to, trust me on that, but if you did, you could definitely distinguish it from the other chems. Randy
S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 25, 2008 #6 I did dissolve with very hot water. SMB.. dont have wiff
P Platdigger Well-known member Supporting Member Joined Jul 26, 2007 Messages 1,662 Location Washington Oct 25, 2008 #7 By wiff, I meant "smell". Don't put your nose too close.....that stuff is bad. If there was no smell, sounds to me like you have one of the other chemicals. Randy
By wiff, I meant "smell". Don't put your nose too close.....that stuff is bad. If there was no smell, sounds to me like you have one of the other chemicals. Randy
S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 25, 2008 #8 it is very bad I dont smel it cuz it is bad