Hello all! I’m back with another question/concern I have regarding silver extraction. I’ve successfully made my first two .5 gram gold buttons in the last couple weeks (yay!) and in the process of making those two I’ve been encountering a bunch of white/gray powder in my filters that I suspect is silver? When I dilute the aqua Regis with water it seems to form which leads me to think it actually is silver??
I’m not exactly sure but it doesn’t dissolve in aqua Regia, I’ve processed everything in either HCL or Nitric beforehand to remove lead/tin/solder and such, which by the way I mostly deal with e-scrap, so all I know is that it isn’t gold!
I’m heating the powders in some water to see if they dissolve. Here are a few pics of the powders that have been popping up at filtering.
I’m not sure what else to add so please ask me more questions if you need anymore insight as to what keeps popping up. I’m worried it’s a mix of tantalum, platinum, palladium, and silver which I have no experience with, I have a separate jar of liquid from another run I believe is filled with palladium, I just don’t know what to do with it so I set it aside!
I’m not exactly sure but it doesn’t dissolve in aqua Regia, I’ve processed everything in either HCL or Nitric beforehand to remove lead/tin/solder and such, which by the way I mostly deal with e-scrap, so all I know is that it isn’t gold!
I’m heating the powders in some water to see if they dissolve. Here are a few pics of the powders that have been popping up at filtering.
I’m not sure what else to add so please ask me more questions if you need anymore insight as to what keeps popping up. I’m worried it’s a mix of tantalum, platinum, palladium, and silver which I have no experience with, I have a separate jar of liquid from another run I believe is filled with palladium, I just don’t know what to do with it so I set it aside!