Mistakes were made.

Used thiolsulphate to leach gold plated pins, got a clear solution.
Then added hcl to get to a ph of 3-4 and added smb. And then realised smb doesn't work with thiolsulphate.
The solution turned a yellow murky colour, i suspect the ph caused the thiolsuphate to degrade, fine gold in solution, no longer dissolved.
Dunno how to get the gold now?
High salt from both HCL and NaOH that were added to adjust ph, can't tell ph from high salt.
 
Mistakes were made.

Used thiolsulphate to leach gold plated pins, got a clear solution.
Then added hcl to get to a ph of 3-4 and added smb. And then realised smb doesn't work with thiolsulphate.
The solution turned a yellow murky colour, i suspect the ph caused the thiolsuphate to degrade, fine gold in solution, no longer dissolved.
Dunno how to get the gold now?
High salt from both HCL and NaOH that were added to adjust ph, can't tell ph from high salt.
Well HCl and NaOH gives NaCl(Table Salt).
Salt is neutral and should not affect the pH to much I believe.

I'm not sure if SMB works with ThioSulfate or not, but it should be more in the range of 2-1 for best effect.
If the Gold are in particle form just add HCl and a little bit of Bleach and it will redissolve
and you can use SMB, Copperas, Ascorbic or what ever your preferences are.

What you do NOT do is start throwing chemicals at it in hope something works.
Ask first.
 
What would happen if you just evaporate to a powder and furnace it? Dumb idea?
One of the reasons ThioSulfate is not much used is that it is hard to get the Gold out.
Smelting might be a solution but might be riddled with heavy losses.
Not sure here, but smelting/decomposing salts always poses risks of losses.

The best bet is always to use the most common methods, they are most common for good reasons.
 
Another idea is to use the charmin plug basically a toilet paper plug in a funnel , pour your solution through it and it should catch your fine gold particles if you still see particles in the solution you may need to do it again , rinse thoroughly with water , recover the plug and dissolve your gold using Hcl and bleach or HCl and peroxide , filter and precipitate your gold .
 
Another idea is to use the charmin plug basically a toilet paper plug in a funnel , pour your solution through it and it should catch your fine gold particles if you still see particles in the solution you may need to do it again , rinse thoroughly with water , recover the plug and dissolve your gold using Hcl and bleach or HCl and peroxide , filter and precipitate your gold .
Maybe I misunderstood. I thought it still was in solution?
 
Tried adding hcl, went from clear, to murky yellow over a minute, then to orange and then dark orange / brown over minutes.

Think this is fine gold? It may look different to smb precipitated gold as smb grows larger gold particles, in this case it could be very fine.