palladium processing with potassium hydroxide and ammonia

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

angga996

New member
Joined
Sep 22, 2021
Messages
4
Halo semuanya, saya ingin mengajukan beberapa pertanyaan tentang kemurnian paladium yang diperoleh. Menurut saya, cara ini mudah dilakukan dan tidak memakan waktu lama dalam penanganannya.

Langkah pertama saya dalam pemurnian paladium:

1. Saya memasukkan semua bahan yang mengandung paladium, nikel, perak, aluminium dan tembaga di hno3.
2. Saya menambahkan kalium hidroksida(KOH) untuk memfasilitasi pemurnian lebih lanjut.
3. Saring dan tambahkan hcl untuk mendapatkan paladium dan hilangkan semua jejak termasuk tembaga, dan perak tidak termasuk nikel, tapi saya bukan yang menggunakan aluminium, apakah mereka menggunakan larutan HCL atau mengendap di dasar.
4. Saya menggunakan kalium hidroksida untuk mengembalikannya ke dalam larutan HCL.
5. Menambahkan amonia ke paladium dan nikel yang diperoleh dari kalium hidroksida (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke dalam spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah dasarnya.

Terima kasih untuk kalian semua.
 
Could you please post that in English.
Not many read your language here.
Malay is it?
Regards Per-Ove
 
Halo semuanya, saya ingin mengajukan beberapa pertanyaan tentang kemurnian paladium yang diperoleh. Menurut saya, cara ini mudah dilakukan dan tidak memakan waktu lama dalam penanganannya.

Langkah pertama saya dalam pemurnian paladium:

1. Saya memasukkan semua bahan yang mengandung paladium, nikel, perak, aluminium dan tembaga di hno3.
2. Saya menambahkan kalium hidroksida(KOH) untuk memfasilitasi pemurnian lebih lanjut.
3. Saring dan tambahkan hcl untuk mendapatkan paladium dan hilangkan semua jejak termasuk tembaga, dan perak tidak termasuk nikel, tapi saya bukan yang menggunakan aluminium, apakah mereka menggunakan larutan HCL atau mengendap di dasar.
4. Saya menggunakan kalium hidroksida untuk mengembalikannya ke dalam larutan HCL.
5. Menambahkan amonia ke paladium dan nikel yang diperoleh dari kalium hidroksida (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke dalam spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah dasarnya.

Terima kasih untuk kalian semua.
Proses pertama harus melarutkan bahan baku dan semen paladium ke tembaga padat berat. Menambahkan udara ke gelembung melalui larutan akan mengaduk dan membantu mengoksidasi tembaga. Ini memaksa paladium keluar dari larutan. Prosesnya bisa memakan waktu tetapi Anda memiliki stok yang jauh lebih bersih untuk dikerjakan. Paladium akan menjadi bubuk halus hitam dari paladium logam. Bubuk dikumpulkan dan dibilas dengan air dan kemudian dilarutkan kembali untuk pemurnian lebih lanjut.
 
Halo semuanya, saya ingin mengajukan beberapa pertanyaan tentang kemurnian paladium yang diperoleh. Menurut saya, cara ini mudah dilakukan dan tidak memakan waktu lama dalam penanganannya.

Langkah pertama saya dalam pemurnian paladium:

1. Saya memasukkan semua bahan yang mengandung paladium, nikel, perak, aluminium dan tembaga di hno3.
2. Saya menambahkan kalium hidroksida(KOH) untuk memfasilitasi pemurnian lebih lanjut.
3. Saring dan tambahkan hcl untuk mendapatkan paladium dan hilangkan semua jejak termasuk tembaga, dan perak tidak termasuk nikel, tapi saya bukan yang menggunakan aluminium, apakah mereka menggunakan larutan HCL atau mengendap di dasar.
4. Saya menggunakan kalium hidroksida untuk mengembalikannya ke dalam larutan HCL.
5. Menambahkan amonia ke paladium dan nikel yang diperoleh dari kalium hidroksida (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke dalam spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah dasarnya.

Terima kasih untuk kalian semua.

angga996 wrote :
"​

Hello everyone, I would like to ask you a few questions about the purity of the palladium obtained. In my opinion, this method is easy to do and does not take long to handle.

My first steps in refining palladium:

1. I included all materials containing palladium, nickel, silver, aluminum and copper in hno3.
2. I added potassium hydroxide(KOH) to facilitate further purification.
3. Filter and add hcl to get palladium and remove all traces including copper, and silver excluding nickel, but I'm not the one using aluminum, whether they use HCL solution or settle to the bottom.
4. I used potassium hydroxide to return it to the HCL solution.
5. Adding ammonia to palladium and nickel obtained from potassium hydroxide (KOH).
6. I put HCL in ammonia solution to get a bright yellow sponge.

What I want to ask is how much purity do I get this way?

Does the ammonia simply precipitate the palladium and leave traces of nickel in the solution or does it still carry over into the palladium yellow sponge?

What about aluminum, do they dissolve with HCL or just stay under the base.

Thanks to all of you."
 
I answered :
"The first process must dissolve the raw material and palladium cement into heavy solid copper. Adding air to the bubbles through the solution will stir and help oxidize the copper. This forces the palladium out of solution. The process can take some time but you have much cleaner stock to work with. Palladium will be a black fine powder of metal palladium. The powder is collected and rinsed with water and then redissolved for further purification."
 
There seems to be a slight problem with the language I'm using,...
Thank you for reminding me.

"Hello everyone, I would like to ask you a few questions about the purity of the palladium obtained. In my opinion, this method is easy to do and does not take long to handle.

My first steps in refining palladium:

1. I included all materials containing palladium, nickel, silver, aluminum and copper in hno3.
2. I added potassium hydroxide(KOH) to facilitate further purification.
3. Filter and add hcl to get palladium and remove all traces including copper, and silver excluding nickel, but I'm not the one using aluminum, do they use HCL solution or settle to the bottom.
4. I used potassium hydroxide to return it to the HCL solution.
5. Adding ammonia to palladium and nickel obtained from potassium hydroxide (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah alasnya.

Terima kasih untuk kalian semua."

Saya menyalin utas di atas dan mengubah ke bahasa Inggris. Semoga bisa dipahami isinya.

Terima kasih
 
“Halo semuanya, saya ingin menanyakan beberapa pertanyaan tentang kemurnian paladium yang diperoleh. Menurut saya, cara ini mudah dilakukan dan tidak membutuhkan waktu lama untuk menanganinya.

Langkah pertama saya dalam pemurnian paladium:

1. Saya memasukkan semua bahan yang mengandung paladium, nikel, perak, aluminium dan tembaga di hno3.
2. Saya menambahkan kalium hidroksida(KOH) untuk memudahkan pemurnian lebih lanjut.
3. Saring dan tambahkan hcl untuk mendapatkan paladium dan hilangkan semua jejak termasuk tembaga, dan perak tidak termasuk nikel, tapi saya bukan yang menggunakan aluminium, apakah mereka menggunakan larutan HCL atau mengendap di bawah.
4. Saya menggunakan kalium hidroksida untuk mengembalikannya ke larutan HCL.
5. Menambahkan amonia ke paladium dan nikel yang diperoleh dari kalium hidroksida (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah alasnya.

Terima kasih untuk kalian semua."
 
“Halo semuanya, saya ingin menanyakan beberapa pertanyaan tentang kemurnian paladium yang diperoleh. Menurut saya, cara ini mudah dilakukan dan tidak membutuhkan waktu lama untuk menanganinya.

Langkah pertama saya dalam pemurnian paladium:

1. Saya memasukkan semua bahan yang mengandung paladium, nikel, perak, aluminium dan tembaga di hno3.
2. Saya menambahkan kalium hidroksida(KOH) untuk memudahkan pemurnian lebih lanjut.
3. Saring dan tambahkan hcl untuk mendapatkan paladium dan hilangkan semua jejak termasuk tembaga, dan perak tidak termasuk nikel, tapi saya bukan yang menggunakan aluminium, apakah mereka menggunakan larutan HCL atau mengendap di bawah.
4. Saya menggunakan kalium hidroksida untuk mengembalikannya ke larutan HCL.
5. Menambahkan amonia ke paladium dan nikel yang diperoleh dari kalium hidroksida (KOH).
6. Saya memasukkan HCL ke dalam larutan amonia untuk mendapatkan spons kuning cerah.

Yang ingin saya tanyakan adalah berapa banyak kemurnian yang saya dapatkan dengan cara ini?

Apakah amonia hanya mengendapkan paladium dan meninggalkan jejak nikel dalam larutan atau masih terbawa ke spons kuning paladium?

Bagaimana dengan aluminium, apakah mereka larut dengan HCL atau hanya tinggal di bawah alasnya.

Terima kasih untuk kalian semua."
"Hei alle sammen, jeg vil gjerne stille noen spørsmål om renheten til det oppnådde palladiumet. Etter min mening er denne metoden enkel å gjøre og tar ikke lang tid å håndtere.

Mitt første trinn i palladiumrensing:

1. Jeg inkluderte alle materialer som inneholder palladium, nikkel, sølv, aluminium og kobber i hno3.
2. Jeg tilsatte kaliumhydroksid (KOH) for å lette videre rensing.
3. Sil og tilsett hcl for å få palladium og fjern alle spor inkludert kobber, og sølv ikke inkludert nikkel, men jeg er ikke den som bruker aluminium, enten de bruker HCL-løsning eller legger seg på bunnen.
4. Jeg bruker kaliumhydroksid for å returnere det til HCL-løsningen.
5. Tilsett ammoniakk til palladium og nikkel oppnådd fra kaliumhydroksid (KOH).
6. Jeg legger HCL i ammoniakkløsningen for å få en knallgul svamp.

Alt jeg vil spørre er hvor mye renhet jeg får på denne måten?

Utfeller ammoniakken bare palladium og etterlater spor av nikkel i løsningen, eller blir den fortsatt ført bort til den gule svampen av palladium?

Hva med aluminium, løser de seg opp i HCL eller holder seg bare under basen.

Takk for dere alle sammen."

Hvorfor nøytraliserer du løsningen med KOH?
Hvis du bruker KCl.
Beholder du Ph som den er.
En annen ting er at oversettelsen blir rar og utydelig, noe som kan være farlig når en bruker kjemikalier.

Hi Angga!
Can you now see how difficult it can be to help you?
Unless you want help only from you country, it may be wise to post in English.
Another thing is that you now have at least 3 threads with more or less the same question. Which is strictly against rules. Can one of the mods merge these threads please.

Regards Per-Ove
 