Just to test theory I am soaking about a teaspoon of header pins in 3oz of hcl and 1 oz of peroxide(3%), with no heat I know this will take a while. my question is will this dissolve any gold after all other metals are gone? If it does can it be percipitated with smb.

Does it make a difference if the peroxide is added in smaller amounts more frequently.

I have a few other jars of the same solution with different types of pins, and contacts as not to mix materials


first post
thanx for this board.
 
lmills,

Welcome to the forum,

Excellent strategy!!! I like the way you think.

The ratio you specified of 3:1 is not what I recommend, but it's not a bad idea. The lower concentration of peroxide will have a much harder time dissolving any gold so that shouldn't be a problem until you pass the 2:1 ratio with peroxide additions (Acid:peroxide). If you keep the temperature at room temperature (25 C )you shouldn't have any gold absorbed.

Any absorbed gold will readily percipitate using SMB. It's a little harder to see the percipitation with the dark green color of the solution, it will appear as a slight darkening of the solution within minutes of adding the SMB. After about 30 minutes or so you'll start to notice the bottom of the beaker getting a dark tint to it, that's the gold dropping to the bottom. I wait overnight before pouring off and rinseing.

Keep us posted.

Steve