I use 60% peroxide to destroy sulfur complexes of gold in the lab. Usually, high concentrated peroxide contains acidic stabilizers to avoid fast decompose. And of course, you need to store it under 15C.
Can you tell me how you applied it and how long you waited? Thank you.
 