In a few words if I put 15 grams of silver nitrate powder in 250 ml distilled water will it start the cementation ?
Let us back up a little.In a few words if I put 15 grams of silver nitrate powder in 250 ml distilled water will it start the cementation ?
In light of 4Metals comment I want to ask a question.In a few words if I put 15 grams of silver nitrate powder in 250 ml distilled water will it start the cementation ?
At the moment I just want to create a solution that will start the silver cementation from copper , just to see if I can make it , this will be my very first attempt, by the way thank you for digging deep into it , do you think if I dissolve 25 grams of silver nitrate powder in 500ml of distilled water and I place a copper bar into the silver nitrate liquid solution , will it start the cementation ? Regarding the electrolyte for the silver cell I saw I very well explain video from sreetips on YouTube , he also did a video on how to make a silver nitrate from a silver bar to then use it as a solution to deep the copper and obtain the silver cement , I just didn’t want to get involve with dangerous yellow fumes ( it’s my very first time )Let us back up a little.
You want to set up a Silver cell to refine Silver?
Then you need an Electrolyte with Silver Nitrate.
The size of the cell dictates how much electrolyte you need and then the concentration then tells how much in grams you need.
I believe 25 grams is way to little.
Then you need a feed stock which usually are fine Silver or Sterling that are in the form of shots or bar.
Then you need a Power source for your cell.
The electrolyte needs to be monitored and replenished form time to time and it need a bit of surplus Nitric to do that.
The cell also needs to be monitored and emptied from time to time to avoid the cell to short out.
How much material do you have to process?
Cementing is what you do when the cell is finished with its work and you need to rejuvenate the electrolyte.
Thank you I only have 25 grams of silver nitrate powdersolubility of silver nitrate is 256 g/100 mL at (25 °C)
So maybe a 25 ml of distilled water in a 50 ml beaker would be ok
Just use a 1/4 inch to 1/2 copper coupling to cement out the silver
Dissolve it in water and add a little Nitric and you are ready to go.At the moment I just want to create a solution that will start the silver cementation from copper , just to see if I can make it , this will be my very first attempt, by the way thank you for digging deep into it , do you think if I dissolve 25 grams of silver nitrate powder in 500ml of distilled water and I place a copper bar into the silver nitrate liquid solution , will it start the cementation ? Regarding the electrolyte for the silver cell I saw I very well explain video from sreetips on YouTube , he also did a video on how to make a silver nitrate from a silver bar to then use it as a solution to deep the copper and obtain the silver cement , I just didn’t want to get involve with dangerous yellow fumes ( it’s my very first time )
Which is to little for anything else than experimenting.Thank you I only have 25 grams of silver nitrate powder
Thank you I will definitely follow the adviseFlatting it is more correct really some times I flatten some times I don’t , make sure it clean .
Good luck
When cementing on copper metal a slab is best because as it thins out you notice it and you can stop using it by the time little bits of coper break off and mix with your Silver metal. Copper pipe, being thinner, does not last as long. The copper in with your Silver metal doesn't hurt the cell but as it builds up it has to be removed or it will co-deposit and lower the purity of your Silver from the cell. A little copper in the cell actually helps the crystal structure grow. But since most cells today run on sterling Silver there is never a shortage of copper, so why let sloppy technique increase the copper content of your cement Silver when it doesn't have to?Flatting it is more correct really some times I flatten some times I don’t , make sure it clean .
To make a silver cell electrolyte? That's a simple one: Enough for it all to dissolve, then you have a saturated solution, which is too strong for the electrolyte. so add more distilled water.I was looking for the silver nitrate powder to liquid ratio but I guess it’s way to hard to get this answer , thanks anyway , sorry I didn’t know that was difficult
Why did you quote my message? i did not get the purpose of it or the question you may have.I think you are making it a little hard on yourself , to me this not practical, You don’t want to make silver nitrate but buy it for cementation and for your silver cell. You goal is to make silver bars or shot
Things needed
Silver nitrate for cementation
Torches to melt the Impure silver
Melt dishes to cast shot or bars
Mold to make bar
Silver feed stock for cell
Silver nitrate for cell
Hand tools
Power supply
Why not just buy silver bars ?
Do you have any impure silver to refine? if not this makes no sense. What did you pay for the 99.99% pure silver nitrate?what I would like is to make a liquid silver nitrate solution ( but I bought a silver nitrate 99.99% 25gr powder , and I don’t know how much water I need to add to make it a liquid solution , with the liquid solution I would like to put inside a copper bar and obtain silver cement powder , with the cement powder I would like to melt it into a bar or make a silver shot to start a silver cell
There are a lot of questions to the intention and plans or lack thereof from this poster.Do you have any impure silver to refine? if not this makes no sense. What did you pay for the 99.99% pure silver nitrate?
Martijn my phone froze up I had to back out of the screen then return back to finish typing I didn’t know it copied you post . Heck maybe I hit quote it by accidentWhy did you quote my message? i did not get the purpose of it or the question you may have.
Enter your email address to join: