Preparing for Christmas

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
I love my 5L but hate being limited to 3.5L for my reactions as that's my limit for safety. I've went bigger a few times and it gets VERY sketchy and I've foamed over, loosing 1/3 of it a few times.
Transition from 5 L beaker to reactors (proper, expensive way of executing larger reactions) or plastic barrels is always sobering :) It does not seem like a big deal to do say AR dissolution in cut HDPE canister, but it is very different. Once you tackle down the main problem - how to heat the contents without destruction of temperature sensitive HDPE - you practically won.

Biggest reaction I ever watched was in 220 L HDPE barrel. Foam over on this scale is something vastly different comparing to 5 L beaker. By the time you realize that you sometimes even need some sort of blower or vacuum suction tube to suck NOx-es from the space in the barrel unoccupied by liquid - because they are so dense that you can leave it open in hood for one hour and still see just brown... :)
And also, pouring solution with 100 ozt of gold or palladium by hand from relatively fragile 22L glass round bottom... That can result in horrible financial disaster if you somehow manage to screw up :)
Yeah, it is very different.

PS: Never lift HDPE vessel with hot contents :) always let it cool properly and after two or three dissolutions, replace it with new one. AR can do extraordinary damage, even to HDPE. Siphoning or pumping is preferred over pouring.
 
By the time you realize that you sometimes even need some sort of blower or vacuum suction tube to suck NOx-es from the space in the barrel

One of my memories from bucket refining is watching a reaction rise and saying to myself “big bubbles, big bubbles” as if the solution understood me! When the bubbles get big the rise slows down, it’s the small bubble foam that rises with a vengeance. When I saw that coming I was there with a suction receiver and a wand to prevent a disaster. (This is a little trick you learn the hard way!)
 
Nice chemistry set. Be careful and please share photos of some of your setups. Happy New Year.
Here is one for HCl production from waste H2SO4 and NaCl. Double backflow trap. Connections still need to be lubricated with molykote and fixed with clamps.
Hose to the funnel is still loose and I will put the beaker in an ice dish.
Setup to fill, empty and refill without taking it apart.

Not sure if the thermometer is needed, but i will first go for 2Molar in 500ml by converting 60grams of salt.
Tritation will tell how well I did.
Edited to add the picture.
20250112_173139.jpg
 
Not sure if the thermometer is needed,

Those thermometer adapters are fine for most distillations, except for nitric acid. After a few nitric distillations the O-ring that holds the thermometer in place will start to become brittle, followed shortly be the plastic screw cap. I would inspect them after each use and replace them if in doubt.

I'm not 100% sure whether these O-ring/caps are universal or not, but I typed "thermometer adapter replacement" into Amazon and a couple options came up.
 
Oh, you young pups just having grandkids... Enjoy them while you can! We just completed our annual Christmas Eve with the family. Our youngest grandson is 19 and a freshman in college. Our older is living his best life in Colorado. We passed the phone around to everyone to talk to him. Enjoy them while you can!!! Because tomorrow, they'll be grown.

Best wishes to everyone!

Dave
Would you like to adopt a couple more ?
 
I managed to get a 1.1Molar HCl acid, and have added more salt and acid to go for a lot stronger.
A cool thing is you can balance the gas production by adjusting the heating to a point where you can see the chlorine be absorbed by the water and falling to the bottom like a waterfall, and no bubbles escape the inverted funnel, so all the gas produced is dissolved. No losses. Awesome.
Having a great time playing with it!
20250114_223324.jpg
Great use for waste sulfuric and I can't wait to use my first homemade HCl.
 
I managed to get a 1.1Molar HCl acid, and have added more salt and acid to go for a lot stronger.
A cool thing is you can balance the gas production by adjusting the heating to a point where you can see the chlorine be absorbed by the water and falling to the bottom like a waterfall, and no bubbles escape the inverted funnel, so all the gas produced is dissolved. No losses. Awesome.
Having a great time playing with it!
View attachment 66509
Great use for waste sulfuric and I can't wait to use my first homemade HCl.
What a great way to recycle the sulfuric acid from the stripping cell. I really like that hood did you steam the wood to make that curved front ?
 
I just tritated the end result and had to add 27 gr of 1M NaOH to 4.88 gr of HCl.
I calculated that is about 6.3M or a bit over 20% HCl. Good enough for washing powder clean and strong AR.
I have added more than 10 Mol of salt to make most use of my sulfuric. I rather waste salt than acid.

There was a small pool of high concentrated HCl in the catch bottle which i added after tritation, so I think it is at or above at least 20%

More black powder was collected from evaporating the sulfuric waste and i will process that with my fresh acid.
Edited for spelling.
 
I just tritated the end result and had to add 27 gr of 1M NaOH to 4.88 gr of HCl.
I calculated that is about 6.3M or a bit over 20% HCl. Good enough for washing powder clean and strong AR.
I have added more than 10 Mol of salt to make most use of my sulfuric. I rather waste salt than acid.

There was a small pool of high concentrated HCl in the catch bottle which i added after tritation, so I think it is at or above at least 20%

More black powder was collected from evaporating the sulfuric waste and i will process that with my fresh acid.
Edited for spelling.
It is close the azeotrope so that makes sense.
If you aim to go over azeotropic concentration you need vacuum distillation or similar.
 
It is close the azeotrope so that makes sense.
If you aim to go over azeotropic concentration you need vacuum distillation or similar.
I think if i keep generating chlorine gas it will stil be absorbed by the water and the concentration wil keep rising over the azeotropic point.
You can not increase the concentration of an azeotropic muxture by destillation, this is because at the azeotrope, it behaves as a single solution and vapor.
But you can add more chlorine or even extract water by adding a strong dehydrating agent.
Screenshot_20250118_215853_Chrome.jpg
At 38% the boiling point is only 48C and the high vapor pressure will cause a lot of fuming.
But at 32% it is a good strong acid.
I think 32% was the strenght I bought it at when it was still available for me.
I will keep buying 10% for dirty AR. And I can always make one liter stronger when i need to.
 
I think if i keep generating chlorine gas it will stil be absorbed by the water and the concentration wil keep rising over the azeotropic point.
You can not increase the concentration of an azeotropic muxture by destillation, this is because at the azeotrope, it behaves as a single solution and vapor.
But you can add more chlorine or even extract water by adding a strong dehydrating agent.
View attachment 66576
At 38% the boiling point is only 48C and the high vapor pressure will cause a lot of fuming.
But at 32% it is a good strong acid.
I think 32% was the strenght I bought it at when it was still available for me.
I will keep buying 10% for dirty AR. And I can always make one liter stronger when i need to.
I think I said that wrong, for HCl one need to distill under pressure not vacuum.
But it still need "specialized" equipment.

Industrially they use a third agent to push the equilibrium.
Maybe molecular sieves can be used?
 
Now testing 100 grams of ammonium nitrate in the sulfuric waste.

The temperature is 120 degrees in the bend, so i'm expecting azeotropic 68% HNO3.
Man i love this lab set!
Scraping the last bits of black gold powder from the evaporation dishes to process with my home made AR.
some foils from AP..
I'm so glad I found this forum long ago and learned chemistry.
 

Attachments

  • 20250119_024953.jpg
    20250119_024953.jpg
    1.2 MB