at the end of lazersteve's video it states ""now your ready for clorox & acid""

is there a video or info that continues the process of Processing Fingers in AP and the use of "clorox & acid" to clean up the flake / copper .....

thank you
 
There is a video of steve dissolving the foils in HCl + chlorox.

HCl + Chlorox will dissolve gold and base metals, once done, your next step is to filter the gold solution, warm it to 67-70C for few minutes to eliminate excess Cl2. Then drop the gold with SMB
 
samuel-a said:
There is a video of steve dissolving the foils in HCl + chlorox.

HCl + Chlorox will dissolve gold and base metals, once done, your next step is to filter the gold solution, warm it to 67-70C for few minutes to eliminate excess Cl2. Then drop the gold with SMB



very helpful thank you very much

its just the videos never stop buffering ??

win7 ultimate 64 bit w/ IE9 X64

going to try my old laptop to see if i can view with win XP 32bit IE8 X32

thanks again samuel-a
 
No need to wait for videos buffering. You can buy videos in high quality on dvd from Steve for very reasonable price. You will have them at your disposal anytime you want to see process again.
 
patnor1011 said:
No need to wait for videos buffering. You can buy videos in high quality on dvd from Steve for very reasonable price. You will have them at your disposal anytime you want to see process again.


patnor1011, glorycloud do you own any of the lazersteve videos ?
do you buy from his store ??

if so i will buy, watch and then post.

what i would like to do is:

see if it is something i can do in my location without spending $100,000 on filtered rooms & lab equipment.

the pm's i am thinking of processing are coming from 100% consumer electronics

is there a "how to" for refining pm's from "100% consumer electronics"

does lazersteve have what i need in his videos?

i did not see a "this video contains" on his site, i only see a brief discription & a semi stocked store with some refining products & that makes me wonder........
spoons for sale..... bowls for sale ...... but no soup for sale ??

i dont mind spending $25.00 to have a good education
but i need to ask about the answers that are not there, i would like to think that some of the posts lazersteve has written mite be more usefull on his site ?

and more info about the contents of his vids would be great also

maybe eash person here that owns it can write a little something about each video so he can put it on his site so people like me can read that & ponder the thought of:

"is that what i was looking for"

signed....
its easy to buy & hard to sell

Dave from canada
 
necromancer said:
patnor1011 said:
No need to wait for videos buffering. You can buy videos in high quality on dvd from Steve for very reasonable price. You will have them at your disposal anytime you want to see process again.


patnor1011, glorycloud do you own any of the lazersteve videos ?
do you buy from his store ??

if so i will buy, watch and then post.

what i would like to do is:

see if it is something i can do in my location without spending $100,000 on filtered rooms & lab equipment.

the pm's i am thinking of processing are coming from 100% consumer electronics

is there a "how to" for refining pm's from "100% consumer electronics"

does lazersteve have what i need in his videos?

i did not see a "this video contains" on his site, i only see a brief discription & a semi stocked store with some refining products & that makes me wonder........
spoons for sale..... bowls for sale ...... but no soup for sale ??

i dont mind spending $25.00 to have a good education
but i need to ask about the answers that are not there, i would like to think that some of the posts lazersteve has written mite be more usefull on his site ?

and more info about the contents of his vids would be great also

maybe eash person here that owns it can write a little something about each video so he can put it on his site so people like me can read that & ponder the thought of:

"is that what i was looking for"

signed....
its easy to buy & hard to sell

Dave from canada

Dave, I only answer first question and it is Yes. You only need to spend more time here, read more and then you will understand. If there will not be people like Steve around who is here from start giving away help and information for free we would never be here. You are about to get free education here, in topics which were closely guarded secret of few chosen people not long time ago.
Answer on all your questions is here on this forum. Steves videos will help you visualize information you gain studying. He is that guy who showed us how to use AP process you talk about.
 
As you will find most of processing is mainly spending time to prepare materials. Actual chemicals involved are not that expensive. You really want to invest in proper safety measures as accidents happen mostly when we dont expect them.
What material you want to process?
 
patnor1011 said:
As you will find most of processing is mainly spending time to prepare materials. Actual chemicals involved are not that expensive. You really want to invest in proper safety measures as accidents happen mostly when we dont expect them.
What material you want to process?


i am thinking to refine (fingers, flatpacks & mcc) to start

i have a small amount that i have processed over the last few days
will send pics soon

thank you
 
I own three of Steve's fine DVD's and have donated more than once to
his fine website in addition to buying products from Steve.

If one of ten lurkers and occasional posters would buy something
from or donate to Steve's website as a small thank you for all
his time and effort freely given to so many of us, it would simply
be a small way to say "thank you"!

I have ordered GSP's fine material as well and have sent a processor
to our esteemed professor Harold. Why? It's all about the Golden Rule:
"Do unto others as you would have them do unto you". 8)
 
glorycloud said:
I own three of Steve's fine DVD's and have donated more than once to
his fine website in addition to buying products from Steve.

If one of ten lurkers and occasional posters would buy something
from or donate to Steve's website as a small thank you for all
his time and effort freely given to so many of us, it would simply
be a small way to say "thank you"!

I have ordered GSP's fine material as well and have sent a processor
to our esteemed professor Harold. Why? It's all about the Golden Rule:
"Do unto others as you would have them do unto you". 8)


you forgot Golden Rule number 2:

kindness begets kindness.

i have been sent some private messages, i am sure i will place some orders from steve

i also think i will ask him to expand his store (ebay sucks)

thank you for your responce sir !!
 

Latest posts

Back
Top